Current location - Education and Training Encyclopedia - Graduation thesis - How to deal with orange peel and pinhole on the workpiece during cathodic electrophoresis?
How to deal with orange peel and pinhole on the workpiece during cathodic electrophoresis?
The main reasons for the roughness of electrophoretic surface are as follows:

1, Yan-base ratio is too high; 2. The paint does not dissolve well; 3. Too much acid in the anolyte system; 4, the intermittent time between the workpiece out of the groove and cleaning is too long; 5. The flushing area is polluted.

The main treatment methods are as follows:

1, adjusted by adding resin; 2. Adding glacial acetic acid or sulfamic acid to adjust the PH value and change the feeding speed; 3. Adding PH regulator to increase the conductivity of anode solution; 4. Adjust the spraying time of the nozzle on the cleaning tank; 5. Reduce the solid content in the rinsing liquid or filter the rinsing liquid.